bdyman has a reputation beyond reputebdyman has a reputation beyond reputebdyman has a reputation beyond reputebdyman has a reputation beyond reputebdyman has a reputation beyond reputebdyman has a reputation beyond reputebdyman has a reputation beyond reputebdyman has a reputation beyond reputebdyman has a reputation beyond reputebdyman has a reputation beyond reputebdyman has a reputation beyond repute
CORRECTION, WHEN A METAL FLAKE IS APPLIED WE DO NOT SAND METAL FLAKE, OR SAND A MID COAT CLEAR

is this going to be PPG harliquien?? or house of kolor, ppg clear can go over house of kolor, and thats it nothing else can go over that product, i tried and i failed learned my lesson

once a pearl or metal flake is mixed with mid coat clear like ppgs dbu or dbc 500, the way it goes on is the way it looks, no sanding never sand mid coat clear,

3 coats of clear is enough with todays high soild clear, remember 1-1 1/2 coats are sanded off, 1 more coat is buffed off leaving you wil 1 coat of clear

should i put more claer on to avoid this??? NO!!!!! 4 coats the clear starts to look cloudy, orange peel gets to heavy, runs, solvent pop, wrinkling, 3 coats is the perfect number